报道了高功率、高效率单模中红外2.8 μm 波段光纤激光器。采用中心波长为975 nm 的半导体激光器(LD)抽运高掺铒氟化物双包层光纤Er∶ZBLAN,室温下实现了2.8 μm激光功率超过9 W中红外光纤激光连续输出。激光器最大输出功率为9.2 W,斜率效率为24.8%,工作阈值约为1.0 W,中心波长为2.79 μm,激光工作模式为单模,光束质量M2因子小于1.2。

Abstract

A high power and high efficiency mid-infrared at 2.8 μm single mode fiber laser is demonstrated. Output power of exceeding 9 W from heavily Er3 +-doped ZBLAN double-clad fiber pumped by a laser-diode (LD) centered at 975 nm is obtained in continuous wave regime. The experimental results indicate that the maximum output power of the fiber laser is 9.2 W corresponding to the slope efficiency of 24.8%. Moreover, the threshold and the center wavelength are around 1.0 W and 2.79 μm, respectively. The fiber laser is in single mode operation, with beam quality factor M2 of less than 1.2.

投稿润色
补充资料

中图分类号:TN212;TN248.1

DOI:10.3788/cjl201542.0502008

所属栏目:激光物理

基金项目:激光与物质相互作用国家重点实验室基金(SKLLIM1309)

收稿日期:2014-12-26

修改稿日期:2015-01-16

网络出版日期:--

作者单位    点击查看

沈炎龙:西北核技术研究所激光与物质相互作用国家重点实验室, 陕西 西安 710024
黄珂:西北核技术研究所激光与物质相互作用国家重点实验室, 陕西 西安 710024
周松青:西北核技术研究所激光与物质相互作用国家重点实验室, 陕西 西安 710024
栾昆鹏:西北核技术研究所激光与物质相互作用国家重点实验室, 陕西 西安 710024
朱峰:西北核技术研究所激光与物质相互作用国家重点实验室, 陕西 西安 710024
谌鸿伟:西北核技术研究所激光与物质相互作用国家重点实验室, 陕西 西安 710024
于力:西北核技术研究所激光与物质相互作用国家重点实验室, 陕西 西安 710024
易爱平:西北核技术研究所激光与物质相互作用国家重点实验室, 陕西 西安 710024
冯国斌:西北核技术研究所激光与物质相互作用国家重点实验室, 陕西 西安 710024
叶锡生:西北核技术研究所激光与物质相互作用国家重点实验室, 陕西 西安 710024

联系人作者:沈炎龙(yanlong_xian@126.com)

备注:沈炎龙(1983—),男,硕士,助理研究员,主要从事高功率激光技术及应用方面的研究。

【1】Wang Pu, Liu Jiang. Progress and prospect on ultrafast Tm-doped fiber lasers at 2 μm wavelength[J]. Chinese J Lasers, 2013, 40(6): 0601002.
王璞, 刘江. 2.0 μm 掺铥超短脉冲光纤激光器研究进展及展望[J]. 中国激光, 2013, 40(6): 0601002.

【2】Chen Hao, Li Jianfeng, Ou Zhonghua, et al.. Progress of mid-infrared fiber lasers[J]. Laser & Optoelectronics Progress, 2011, 48(11): 111402.
陈昊, 李剑锋, 欧中华, 等. 中红外光纤激光器研究进展[J]. 激光与光电子学进展, 2011, 48(11): 111402.

【3】Peng Jue, Wang Weimin, Peng Yuefeng, et al.. Optical parametric amplifier based on PPMgO∶CLN[J]. Chinese J Lasers, 2013, 40(6): 0602004.
彭珏, 王卫民, 彭跃峰, 等. 基于PPMgO∶CLN 的光参量放大器[J]. 中国激光, 2013, 40(6): 0602004.

【4】Tan Gaijuan, Xie Jijiang, Zhang Laiming, et al.. Recent progress in mid-infrared laser technology[J]. Chinese Optics, 2013, 6(4): 501-512.
谭改娟, 谢冀江, 张来明, 等. 中波红外激光技术最新进展[J]. 中国光学, 2013, 6(4): 501-512.

【5】Urquhart P. Review of rare earth doped fibre lasers and amplifiers[J]. Optoelectronics, 1988, 135(6): 385-407.

【6】Hao Liyun, Su Cen, Qi Yunfeng, et al.. Second harmonic generation characteristics of continuous wave all-fiber laser oscillator in PPMgO∶LN[J]. Chinese J Lasers, 2013, 40(6): 0602007.
郝丽云, 苏岑, 漆云凤, 等. 基于PPMgO∶LN 晶体的连续波全光纤激光器倍频特性[J]. 中国激光, 2013, 40(6): 0602007.

【7】Zhu X, Peyghambarian N. High-power ZBLAN glass fiber lasers: review and prospect[J]. Advances in Optoelectronics, 2010, 2010: 1-23.

【8】Zhu X, Jian R, Numerical analysis and experimental results of high-power Er/Pr∶ZBLAN 2.7 μm fiber lasers with different pumping designs[J]. Applied Optics, 2006, 45(27): 7118-7125.

【9】Shi Guanghui. Improved method for semiconductor laser coupling[J]. Chinese Optics, 2013, 6(3): 343-352.
史光辉. 半导体激光耦合新方法[J]. 中国光学, 2013, 6(3): 343-352.

【10】Zhu X, Jain R K. 10-W-level diode-pumped compact 2.78 μm ZBLAN fiber laser[J]. Optics Letters, 2007, 32(1): 26-28.

【11】Tokita S, Murakami M, Shimizu S, et al.. Liquid-cooled 24 W mid-infrared Er:ZBLAN fiber laser[J]. Optics Letters, 2009, 34(20): 3062-3064.

【12】Tokita S, Hirokane M, Murakami M, et al.. Stable 10 W Er∶ZBLAN fiber laser operating at 2.71~2.88 μm[J]. Optics Letters, 2010, 35(23): 3943-3945.

【13】Faucher D, Bernier M, Androz G, et al.. 20 W passively cooled single-mode all-fiber laser at 2.8 μm[J]. Optics Letters, 2011, 36(7): 1104-1106.

【14】Tokita S, Murakami M, Shimizu S, et al.. 12 W Q-switched Er∶ZBLAN fiber laser at 2.8 μm[J]. Optics Letters, 2011, 36(15): 2812-2814.

【15】Wei C, Zhu X, Norwood R A, et al.. Er3+-doped ZBLAN fiber laser Q-switched by Fe∶ZnSe[C]. CLEO, 2012: JW2A61.

【16】Wei C, Zhu X, Wang F, et al.. Graphene Q-switched 2.78 μm Er3+-doped fluoride fiber laser[J]. Optics Letters, 2013, 38(17): 3233-3235.

【17】Huang Yuanfang, Peng Yuefeng, Wei Xingbin, et al.. Watt-level continuous wave 2.8 μm mid-infrared Er∶ZBLAN fiber laser[J]. Chinese J Lasers, 2012, 39(5): 0502007.
黄园芳, 彭跃峰, 魏星斌, 等. 瓦级连续波2.8 μm 中红外Er∶ZBLAN 光纤激光器[J]. 中国激光, 2012, 39(5): 0502007.

【18】Peng Yuefeng, Wei Xingbin, Huang Yuanfang, et al.. Muti-watt-level mid-infrared 2.8 μm fiber laser[C]. The 10th Conference of Opto-Electronics Technology, 2012, GD02-024: 195.
彭跃峰, 魏星斌, 黄园芳, 等. 数瓦级中红外2.8 μm 光纤激光器[C]. 第十届全国光电技术学术交流会, 2012, GD02-024:195.

【19】Shen Yanlong, Huang Ke, Zhu Feng, et al.. Laser diode-pumped watt-level single mode heavily erbium-doped mid-infrared fiber laser[J]. Acta Photonica Sinica, 2014, 43(3): 03014002.
沈炎龙, 黄珂, 朱峰, 等. LD 抽运瓦级单模高掺铒中红外光纤激光器[J]. 光子学报, 2014, 43(3): 03014002.

【20】Liu A, Ueda K. The absorption characteristics of circular, offset, and rectangular double-clad fibers[J]. Optics Communications, 1996, 132(5-6): 511-518.

【21】Zhu Feng, Yu Li, An Xiaoxia, et al.. Spectral-narrowing of XeF(C-A) blue-green laser[J]. High Power Laser and Particle Beams, 2010, 22(11): 2588-2592.
朱峰, 于力, 安晓霞, 等. XeF(C-A)蓝绿激光线宽压缩技术[J]. 强激光与粒子束, 2010, 22(11): 2588-2592.

【22】Ming Hai, Zhang Guoping, Xie Jianping. Opto-Electronics Technology[M]. Hefei: University of Science and Technology of China Press, 2001: 173-176.
明海, 张国平, 谢建平. 光电子技术[M]. 合肥: 中国科学技术大学出版社, 2001: 173-176.

【23】He Yuanxing, Li Xinyang. Analysis of influence of CCD′s nonlinear response characterization on measurement results of focal spot and beam quality[J]. Chinese J Lasers, 2012, 39(4): 0408001.
贺元兴, 李新阳. CCD 光电响应非线性特性对激光远场焦斑测量及光束质量计算的影响[J]. 中国激光, 2012, 39(4): 0408001.

您的浏览器不支持PDF插件,请使用最新的(Chrome/Fire Fox等)浏览器.或者您还可以点击此处下载该论文PDF