中国激光, 2010, 37 (8): 2111, 网络出版: 2010-08-13   

激光冲击处理提高00Cr12合金的疲劳性能

Improving Fatigue Properties of 00Cr12 Alloy by Laser Shock Processing
作者单位
江苏大学 机械学院江苏省光子制造科学与技术省重点实验室,江苏 镇江 212013
摘要
对00Cr12合金耐热钢选用合适的参数进行激光冲击强化(LSP),并对其疲劳极限进行了快速测定。探讨和分析了激光冲击前后00Cr12合金表层残余应力与微观组织的变化对其疲劳寿命的影响。试验结果表明,激光冲击诱使材料表面产生了弹塑性形变,从而在表层产生了残余压应力与高密度位错,有效地提高了疲劳寿命。00Cr12合金试样经激光冲击强化后,寿命是未处理的1.6倍。所选用的Locati阶梯式疲劳试验方法与传统的升降法所得到的结果相比,相对误差较小,可快速地为机械的疲劳设计提供可靠的数据。
Abstract
The 00Cr12 alloy heat-resistant steel was strengthened by laser shock processing (LSP) with appropriate parameters,and its fatigue limitation was measured rapidly. The effects of residual stress and microstructure change of the surface layer of 00Cr12 alloy on its fatigue life were discussed and analyzed before and after LSP. The results showed that elastic-plastic deformation was induced by laser impulse on the material surface,which resulted in residual compressive stress and dislocations of high density in the material surface,so the fatigue life of 00Cr12 alloy was effectively improved by LSP. After LSP,the fatigue life of 00Cr12 alloy was 1.6 times as much as the sample without LSP. Compared with the traditional rising and falling methods,the relative error of the results obtained by Locati multistep method was small. This method could provide reliable data for fatigue design of machines.
参考文献

[1] 毛辉. 00Cr12型铁素体不锈钢焊接热影响区组织与性能研究[D]. 哈尔滨:哈尔滨焊接研究所,2009. 1-3

    Mao Hui. Study on the Microstructures and Properties of HAZ in 00Cr12 Ferrite Stainless Steel[D]. Harbin:Harbin Welding Institute,2009. 1-3

[2] . 航空铝合金材料的两种表面冲击加工技术的比较[J]. 金属热处理, 2004, 29(11): 37-39.

    . Comparison of two kinds of laser shock processing for aerospace aluminum alloys[J]. Heat Treatment of Metals, 2004, 29(11): 37-39.

[3] 张永康,张兴权,周建忠 等. LY12CZ铝合金激光喷丸变形[J]. 中国激光,2006,33(10):1417-1421

    Zhang Yongkang,Zhang Xingquan,Zhou Jianzhong et al.. Deformation of aluminum alloy LY12CZ plate by laser shotpeening [J]. Chinese J. Lasers,2006,33(10):1417-1421

[4] 金属材料疲劳裂纹扩展速率试验方法[S]. GB/T6398-2000-4. 中国标准出版社,2001

    Standard test method for fatigue crack growth rates of metallic materials [S]. GB/T6398-2000-4. Standards Press of China,2001

[5] ASTM. ASTM E8M-04 standard test method for tension testing of metallic materials [S]. ASTM,2004

[6] 张永康,陈菊芳,许仁军. AM50镁合金激光冲击强化实验研究[J]. 中国激光,2008,35(7):1068-1072

    Zhang Yongkang,Chen Jufang,Xu Renjun. Experimental research of laser shock strengthening AM50 magnesium alloy [J]. Chinese J. Lasers,2008,35(7):1068-1072

[7] 桂立丰,曹用涛.机械工程材料测试手册(力学卷)[M]. 沈阳:辽宁科学技术出版社,2001. 396-397

    Gui Lifeng,Cao Yongtao. Handbook of Materials Testing for Mechanical Engineering (Mechanics Volume) [M]. Shenyang:Liaoning Science and Technology Publishing House,2001. 396-397

[8] 曾春华,邹十践. 疲劳分析方法及应用[M]. 北京:国防工业出版社,1991. 27-28

    Zeng Chunhua,Zou Shijian. Fatigue Analysis Methods and Applications[M]. Beijing:National Defense Industry Press,1991. 27-28

[9] 曹子文,邹世坤,刘方军 等. 激光冲击处理1Cr11Ni2W2MoV不锈钢[J]. 中国激光,2008,35(2):316-320

    Cao Ziwen,Zou Shikun,Liu Fangjun et al.. Laser shock processing on 1Cr11Ni2W2MoV martensite steel [J]. Chinese J. Lasers,2008,35(2):316-320

[10] 周建忠,黄舒,赵建飞 等. 激光喷丸强化铝合金疲劳特性的数字化分析[J]. 中国激光,2008,35(11):1735-1740

    Zhou Jianzhong,Huang Shu,Zhao Jianfei et al.. Numerical analysis on fatigue properties of aluminum alloy induced by laser shock peening [J]. Chinese J. Lasers,2008,35(11):1735-1740

[11] . 激光冲击处理对金属微结构及其性能的影响[J]. 材料导报, 2006, 20(6): 1-4.

    . The effects of laser shock processing on microstructure and properties of metal[J]. Materials Review, 2006, 20(6): 1-4.

任旭东, 张田, 张永康, 姜大伟, 陈康敏. 激光冲击处理提高00Cr12合金的疲劳性能[J]. 中国激光, 2010, 37(8): 2111. Ren Xudong, Zhang Tian, Zhang Yongkang, Jiang Dawei, Chen Kangmin. Improving Fatigue Properties of 00Cr12 Alloy by Laser Shock Processing[J]. Chinese Journal of Lasers, 2010, 37(8): 2111.

本文已被 13 篇论文引用
被引统计数据来源于中国光学期刊网
引用该论文: TXT   |   EndNote

相关论文

加载中...

关于本站 Cookie 的使用提示

中国光学期刊网使用基于 cookie 的技术来更好地为您提供各项服务,点击此处了解我们的隐私策略。 如您需继续使用本网站,请您授权我们使用本地 cookie 来保存部分信息。
全站搜索
您最值得信赖的光电行业旗舰网络服务平台!