三聚氰胺-甲醛系凝胶老化过程中的体积收缩影响因素
[1] Hrubesh L W,Poco J F.Thin aerogel films for optical,thermal,acoustic and electronic applications[J].J Non-Crystalline Solids,1995,188:46-53.
[2] 沈军,王珏,吴翔.气凝胶--一种结构可控的新型功能材料[J].材料科学与工程,1994,12(3):1-5.(Shen J,Wang J,Wu X.Aerogels--a type of structure controllable new functional materials.Materials Science and Engineering,1994,12(3):1-5)
[3] Pekala R W.Aerogel-based electronic devices[R].Seminar Talk in Wurzburg University,Germany,1992.
[4] 张林,罗炫,杜凯.ICF靶低密度聚合物多孔材料研究进展[J].材料导报,2002,16(6):48-51.(Zhang L,Luo X,Du K.Progress in research on low-density porous polymer for ICF targets.Materials Review,2002,16(6):48-51)
张勇, 任洪波, 张林, 万小波. 三聚氰胺-甲醛系凝胶老化过程中的体积收缩影响因素[J]. 强激光与粒子束, 2007, 19(8): 1299. 张勇, 任洪波, 张林, 万小波. Solvent effect on volume shrinkage of Melamine-Formaldehyde gel in aging process[J]. High Power Laser and Particle Beams, 2007, 19(8): 1299.