摘要
采用Al-Si粉末对AZ91D镁合金进行了同步送粉激光合金化研究,以期改善镁合金的耐腐蚀性能。讨论了激光加工参数与合金化层几何尺寸的对应关系;采用扫描电镜(SEM)、能谱分析仪(EDS)、X射线衍射仪(XRD)等材料表征手段分析了合金化层显微组织的结构特征。通过阳极极化实验评价了AZ91D镁合金激光合金化组织的腐蚀性能。结果表明,AZ91D镁合金激光合金化表层的耐腐蚀性能明显提高; 剖析了Mg2Si,Al12Mg17,Al3Mg2等金属间化合物(IMC)的耐腐蚀作用。
Abstract
Laser alloying of magnesium alloy AZ91D with direct Al-Si power feeding for improvement of corrosion resistance was investigated. The relationship between laser alloying parameters and dimensions of alloyed layers was studied. The microstructural features of the alloyed layer were characterized by using scanning electronic microscope (SEM), energy disperse spectroscopy (EDS) and X-ray diffraction (XRD). Anodic polarization test was applied to evaluate the corrosion performance of AZ91D alloyed layer, which yielded enhanced corrosion resistance. The contribution of the intermetallic compounds (IMCs) of Mg2Si, Al12Mg17, Al3Mg2 in alloyed layers to corrosion resistance was studied.
参考文献

[1] 陈振华 等 著. 镁合金[M]. 北京:化学工业出版社, 2004

    Chen Zhenhua et al.. Magnesium Alloy [M]. Beijing: Chemical Industry Press, 2004

[2] 宋光玲 著. 镁合金腐蚀与防护[M]. 北京:化学工业出版社, 2006. 20~121

    Song Guangling. The Corrosion and Protect on Magnesium [M]. Beijing: Chemical Industry Press, 2006. 20~121

[3] . E. Gray, B. Luan. Protective coatings on magnesium and its alloys — a critical review[J]. Journal of Alloys and Compounds, 2002, 336: 88-113.

[4] . Galun, A. Weisheit, B. L. Mordike. Laser surface alloying of magnesium base alloys[J]. J. Laser Applications, 1996, 8(6): 299-305.

[5] . Subramanian, S. Sircar, J. Mazumder. Laser cladding of zirconium on magnesium for improved corrosion properties[J]. J. Mater. Sci., 1991, 26: 951-956.

[6] . A. Wang, S. Sircar, J. Mazumder. Laser cladding of Mg-Al alloys[J]. J. Mater. Sci., 1993, 28: 5113.

[7] . M. Yue, A. H. Wang, H. C. Man. Corrosion resistance enhancement of magnesium ZK60/SiC composite by Nd∶YAG laser cladding[J]. Scripta Materialia, 1999, 40(3): 303-311.

[8] . M. Yue, Q. W. Hu, Z. Mei et al.. Laser cladding of stainless steel on magnesium ZK60/SiC composite[J]. Materials Lett., 2001, 47(3): 165-170.

[9] . M. Yue, Z. Mei, H. C. Man. Improvement of the corrosion resistance of magnesium ZM51/SiC composite by laser cladding[J]. J. Mater. Sci. Lett., 2001, 20(16): 1479-1482.

[10] . N. Aung, W. Zhou. Effect of heat treatment on corrosion and electrochemical behaviour of AZ91D magnesium alloy[J]. J. Appl. Electrochemistry, 2002, 32(12): 1397-1401.

[11] Sorin Ignat, Pierre Sallamand, Dominique Grevey. Magnesium alloy laser (Nd∶YAG) cladding and alloying with side injection of aluminum power [J]. Applied Surface Science, 2004, 225(1-4):124~134

[12] . Meia, L. F. Guo, T. M. Yue. The effect of laser cladding on the corrosion resistance of magnesium ZK60/SiC composite[J]. Journal of Materials Processing Technology, 2005, 161(3): 462-466.

[13] J. D. Majumdara, R. Galun, B. L. Mordike et al.. Effect of laser surface melting on corrosion and wear resistance of a commercial magnesium alloy [J]. Materials Science and Engineering A, 2003, 361(1-2):119~129

[14] 刘红宾,王存山,高亚丽 等. 镁合金表面激光熔覆Cu-Zr-Al非晶复合涂层[J]. 中国激光, 2006, 33(5):709~713

    Liu Hongbin, Wang Cunshan, Gao Yali et al.. Laser cladding amorphous composite coating of Cu-Zr-Al on magnesium alloy surface [J]. Chinese J. Lasers, 2006, 33(5):709~713

[15] 黄开金,林鑫,陈池 等. AZ91D镁合金表面激光熔覆Zr-Cu-Ni-Al/TiC复合粉末的组织与磨损[J]. 中国激光, 2007, 34(4):549~554

    Huang Kaijin, Lin Xin, Chen Chi et al.. Microstructure and wear behaviour of laser-clad Zr-Cu-Ni-Al/TiC composites on AZ91D magnesium alloy [J]. Chinese J. Lasers, 2007, 34(4):549~554

[16] 高亚丽,王存山,刘红宾 等. 高功率激光熔凝AZ91HP镁合金组织和性能[J]. 中国激光, 2007, 34(7):1019~1024

    Gao Yali, Wang Cunshan, Liu Hongbin et al.. Microstructure and properties of AZ91HP magnesium alloy treated by high power laser melting [J]. Chinese J. Lasers, 2007, 34(7):1019~1024

[17] W. M. Steen. Laser Material Processing [M]. London: Springer-Verlag Limited, 2003

[18] Alloy Phase Diagrams. ASM Handbook [M]. ASM International, 1992, 3

[19] ASTM G3-89 (Reapproved 2004). Standard Practice for Conventions Applicable to Electrochemical Measurements in Corrosion Testing[S]

李达, 钱鸣, 金昌, 李慧. AZ91D镁合金Al-Si粉末激光合金化及腐蚀性能[J]. 中国激光, 2008, 35(9): 1395. Li Da, Qian Ming, Jin Chang, Li Hui. Laser Alloying of Magnesium Alloy AZ91D with Al-Si Powder and Its Corrosion Performance[J]. Chinese Journal of Lasers, 2008, 35(9): 1395.

本文已被 4 篇论文引用
被引统计数据来源于中国光学期刊网
引用该论文: TXT   |   EndNote

相关论文

加载中...

关于本站 Cookie 的使用提示

中国光学期刊网使用基于 cookie 的技术来更好地为您提供各项服务,点击此处了解我们的隐私策略。 如您需继续使用本网站,请您授权我们使用本地 cookie 来保存部分信息。
全站搜索
您最值得信赖的光电行业旗舰网络服务平台!