一种基于工业CT图像的岩心孔隙率计算方法
[1] Wang Wenjian. CT-based reverse engineering for precision inspection and shape analysis[D]. Cincinnati: University of Cincinnati, 1999: 5-9.
[5] Guo Liping, Cappinteri A, Sun Wei, et al. Measurement and analysis of defects in high-performance concrete with three-dimensional micro-computer tomography[J]. Journal of Southeast University, 2009, 25(1): 83-88.
[7] Peng R D, Yang Y C, Ju Y, et al. Computation of fractal dimension of rock pores based on gray CT images[J]. Chin Sci Bull, 2011, 56(26):2256-2266.
[8] 于艳梅,胡耀青,梁卫国,等. 应用CT技术研究瘦煤在不同温度下孔隙变化特征[J]. 地球物理学报, 2012, 55(2):637-644.(Yu Yanmei,Hu Yaoqing, Liang Weiguo, et al. Study on pore characteristics of lean coal at different temperature by CT technology. Chin J Geohys, 2012, 55(2): 637-644)
[9] 吕兆兴. 孔隙裂隙双重介质逾渗理论及应用研究[D]. 太原: 太原理工大学, 2008: 48-70.(Lü Zhaoxin. The theory and its application of percolation in pore and fracture double-medium. Taiyuan: Taiyuan University of Technology, 2008: 48-70)
[10] 李建胜,王东,康天合. 基于显微 CT 试验的岩石孔隙结构算法研究[J]. 岩土工程学报, 2010, 32(11): 1703-1708.(Li Jiansheng, Wang Dong, Kang Tianhe. Algorithmic study on rock pore structure based on micro-CT experiment. Chinese Journal of Geotechnical Engineering, 2010, 32(11): 1703-1708)
[11] Whitted T. An improved illumination model for shaded display[J]. Communications of the ACM, 1980, 23(6):343-349.
方黎勇, 陈鹏, 陈浩. 一种基于工业CT图像的岩心孔隙率计算方法[J]. 强激光与粒子束, 2014, 26(3): 034008. Fang Liyong, Chen Peng, Chen Hao. A calculation method of core porosity based on industrial CT images[J]. High Power Laser and Particle Beams, 2014, 26(3): 034008.