双层预涂覆对激光熔覆金属陶瓷涂层的影响
[1] Ayers J. D., Tucker T. R.. Particulate TiC hardned steel surface by laser melt injection. Thin Solid Films, 1980, 73: 201~207
[2] Feng Zhigang, Han Zhifan, Zhou Zhirong. Study on crack in laser cladding layer of nodulated cast iron. Transactions of Metal Heat Treatment (金属热处理学报), 1995, 16(1): 31~35 (in Chinese)
[3] Barker T. N., Xin H., Hu C.. Design of surface in situ metal-ceramic composite formation via laser treatment. Mater. Sci. Tech., 1994, 10(6): 536~544
[4] Zhou Xianglin, Ye Yifu, Yu Jinhong et al.. Defect and preventive in ceramic-layer by laser cladding. Hot Working Technology (热加工工艺), 1995, 6: 48~50 (in Chinese)
[5] Cooper K. P., Agers J. D.. The influence of proeessing parameters on the cracking tendency of laser processed composite surfaces. Proc. Cont. ICALEO’87
[6] Shang Lijuan, Zhu Jingpu. Problems and resolving methods in the laser-deposition process. Metal Science and Technology (金属科学与工艺), 1992, 11(2): 65~69 (in Chinese)
[8] Jiang Yongqiu, Lin Ruiyang. Fracture analysis of protective coatings on polymers metals and ceramics. Materials Science Progress (材料科学进展), 1993, 7(6): 513~516 (in Chinese)
许伯藩, 史华忠, 张细菊. 双层预涂覆对激光熔覆金属陶瓷涂层的影响[J]. 中国激光, 1998, 25(8): 763. 许伯藩, 史华忠, 张细菊. Effect of Double-layer Precoating on the Laser Cladding Ceramal Layer[J]. Chinese Journal of Lasers, 1998, 25(8): 763.