中国激光, 2016, 43 (12): 1202010, 网络出版: 2016-12-09   

800 MPa级高强钢光纤激光焊接接头微观结构对硬度及疲劳性能的影响 下载: 585次

Effect of Microstructure on Hardness and Fatigue Properties of 800 MPa High Strength Steel Fiber Laser Weld Joints
作者单位
1 苏州大学沙钢钢铁学院, 江苏 苏州 215021
2 西南林业大学机械与交通学院, 云南 昆明 650224
3 苏州大学激光加工中心, 江苏 苏州 215021
引用该论文

王晓南, 郑知, 曾盼林, 章顺虎, 张敏, 陈长军, 陈文刚. 800 MPa级高强钢光纤激光焊接接头微观结构对硬度及疲劳性能的影响[J]. 中国激光, 2016, 43(12): 1202010.

Wang Xiaonan, Zheng Zhi, Zeng Panlin, Zhang Shunhu, Zhang Min, Chen Changjun, Chen Wengang. Effect of Microstructure on Hardness and Fatigue Properties of 800 MPa High Strength Steel Fiber Laser Weld Joints[J]. Chinese Journal of Lasers, 2016, 43(12): 1202010.

参考文献

[1] Kastensson . Developing lightweight concepts in the automotive industry: taking on the environmental challenge with the SNtt project[J]. Journal of Cleaner Production, 2014, 66, 337-346.

[2] Narasimhan S. Effects of laser welding on formability aspects of advanced high strength steel[D]. Waterloo: University of Waterloo, 2008: 54-101.

[3] Wang J, Yang L, Sun M, et al. Effect of energy input on the microstructure and properties of butt joints in DP1000 steel laser welding[J]. Materials & Design, 2016, 90: 642-649.

[4] Xu W, Westerbaan D, Nayak S S, et al. Microstructure and fatigue performance of single and multiple linear fiber laser welded DP980 dual-phase steel[J]. Materials Science and Engineering A, 2012, 553(36): 51-58.

[5] Jia Q, Guo W, Li W, et al. Microstructure and tensile behavior of fiber laser-welded blanks of DP600 and DP980 steels[J]. Journal of Materials Processing Technology, 2016, 236: 73-83.

[6] Bandyopadhyay K, Panda S K, Saha P, et al. Microstructures and failure analyses of DP980 laser welded blanks in formability context[J]. Materials Science and Engineering A, 2016, 652: 250-263.

[7] Zhang F, Ruimi A, Wo P C, et al. Morphology and distribution of martensite in dual phase (DP980) steel and its relation to the multiscale mechanical behavior[J]. Materials Science and Engineering A, 2016, 659: 93-103.

[8] Saray O, Purcek G, Karaman I, et al. Improvement of formability of ultrafine-grained materials by post-SPD annealing[J]. Materials Science and Engineering A, 2014, 619: 119-128.

[9] Lee J H, Park S H, Kwon H S, et al. Laser, tungsten inert gas, and metal active gas welding of DP780 steel: Comparison of hardness, tensile properties and fatigue resistance[J]. Materials & Design, 2014, 64(9): 559-565.

[10] Parkes D, Westerbaan D, Nayak S S, et al. Tensile properties of fiber laser welded joints of high strength low alloy and dual-phase steels at warm and low temperatures[J]. Materials & Design, 2014, 56(4): 193-199.

[11] Li S, Kang Y, Zhu G, et al. Microstructure and fatigue crack growth behavior in tungsten inert gas welded DP780 dual-phase steel[J]. Materials & Design, 2015, 85: 180-189.

[12] Farabi N, Chen D L, Zhou Y. Fatigue properties of laser welded dual-phase steel joints[J]. Procedia Engineering, 2010, 2(1): 835-843.

[13] Hu Z G, Zhu P, Meng J. Fatigue properties of transformation-induced plasticity and dual-phase steels for auto-body lightweight: Experiment, modeling and application[J]. Materials & Design, 2010, 31(6): 2884-2890.

[14] Parkes D, Xu W, Westerbaan D, et al. Microstructure and fatigue properties of fiber laser welded dissimilar joints between high strength low alloy and dual-phase steels[J]. Materials & Design, 2013, 51(5): 665-675.

[15] Farabi N, Chen D L, Li J, et al. Microstructure and mechanical properties of laser welded DP600 steel joints[J]. Materials Science and Engineering A, 2010, 527(4-5): 1215-1222.

[16] Laird C. The influence of metallurgical structure on the mechanisms of fatigue crack propagation[R]. Philadelphia: Fatigue Crack Propagation, Special Technical Publication 415, ASTM, 1967, 131-168.

[17] 张国栋, 杨新岐, 何鑫龙, 等. 300 M超高强度钢及其电子束焊接接头高周疲劳断裂机制研究[J]. 航空材料学报, 2014, 34(1): 69-75.

    Zhang Guodong, Yang Xinqi, He Xinlong, et al. High cycle fatigue failure mechanism of 300 M ultra-high strength steel and its electron beam welded joints[J]. Journal of Aeronautical Materials, 2014, 34(1): 69-75.

王晓南, 郑知, 曾盼林, 章顺虎, 张敏, 陈长军, 陈文刚. 800 MPa级高强钢光纤激光焊接接头微观结构对硬度及疲劳性能的影响[J]. 中国激光, 2016, 43(12): 1202010. Wang Xiaonan, Zheng Zhi, Zeng Panlin, Zhang Shunhu, Zhang Min, Chen Changjun, Chen Wengang. Effect of Microstructure on Hardness and Fatigue Properties of 800 MPa High Strength Steel Fiber Laser Weld Joints[J]. Chinese Journal of Lasers, 2016, 43(12): 1202010.

本文已被 6 篇论文引用
被引统计数据来源于中国光学期刊网
引用该论文: TXT   |   EndNote

相关论文

加载中...

关于本站 Cookie 的使用提示

中国光学期刊网使用基于 cookie 的技术来更好地为您提供各项服务,点击此处了解我们的隐私策略。 如您需继续使用本网站,请您授权我们使用本地 cookie 来保存部分信息。
全站搜索
您最值得信赖的光电行业旗舰网络服务平台!