强激光与粒子束, 2005, 17 (7): 1016, 网络出版: 2006-04-28   

高钾空心玻璃微球的制备

Fabrication of high molar ration K2O hollow glass microsphere for laser fusion research
作者单位
中国工程物理研究院激光聚变研究中心,四川,绵阳,621900
摘要
以无机化合物为初始原料,选择合理的玻璃溶液配方和成球条件,用液滴法制备出直径200 μm,壁厚2 μm,K2O摩尔分数大于10 %的空心玻璃微球(HGM).利用扫描电镜X射线能量色谱仪对玻璃球壳的组分进行了分析.结果表明,所制备的高钾空心玻璃微球各项技术指标能基本满足神光-Ⅱ物理实验的要求,微球球壳成份实测结果与理论计算结果吻合.
Abstract
With inorganic compounds, hollow glass microsphere (HGM) of above 10% molar ratio K2O was prepared by liquid-droplet method.The glass forming oxides content in solutions and technical conditions of preparing were optimized and selected. The molar ratios of glass forming oxides in shell of HGM were analyzed by means of EDA-X device.The results showed that the diameter, wall-thickness, concentricity and sphericity of HGM satisfied the physical experiments on the SG -II device.Test value of molar ratio of glass forming oxides in HGM were closed to theoretic value.

杜守德, 李波, 师韬, 唐永建. 高钾空心玻璃微球的制备[J]. 强激光与粒子束, 2005, 17(7): 1016. DU Shou-de, LI Bo, SHI Tao, TANG Yong-jian. Fabrication of high molar ration K2O hollow glass microsphere for laser fusion research[J]. High Power Laser and Particle Beams, 2005, 17(7): 1016.

本文已被 1 篇论文引用
被引统计数据来源于中国光学期刊网
引用该论文: TXT   |   EndNote

相关论文

加载中...

关于本站 Cookie 的使用提示

中国光学期刊网使用基于 cookie 的技术来更好地为您提供各项服务,点击此处了解我们的隐私策略。 如您需继续使用本网站,请您授权我们使用本地 cookie 来保存部分信息。
全站搜索
您最值得信赖的光电行业旗舰网络服务平台!