高钾空心玻璃微球的制备
[1] Feaerherd J K, Farnum E H. Micromachining of laser fusion target[J].J Vac Sci Technol ,1981 ,18(3):1284-1285.
[2] 邱龙会,傅依备,王小琳,等.液滴法制备高尺度比玻璃球壳的研究[J].强激光与粒子束,1999,11(4):465-469.
Qiu L H,Fu Y B,Wang X L,et al.Fabrication of hollow glass microspheres with high aspect ratios by liquid droplet method .High Power Laser and Particle Beams, 1999,11(4):465-469.
[3] 胡广才,李怀曾,魏胜,等.玻璃球壳生产工艺研究[J].强激光与粒子束,1995,7(2):183-188 .
Hu G C,Li H Z, Wei S,et al. Research of production techniques about hollow glass microspheres.High Power Laser and Particle Beams , 1995,7(2):183-188.
[4] 壁厚1μm以下薄壁空心玻璃微球生产工艺研究[R].中国国防科技报告,1998.
Du S D. Research of production techniques about hollow glass microsphere with wall-thickness less than 1 micron. Technological Report of China National Defence, 1998.
[5] Compbell J H, Dunsmuir J H. Preparation and properties of hollow glass microspheres for used in laser fusion experiments[R].UCRL-53516.
杜守德, 李波, 师韬, 唐永建. 高钾空心玻璃微球的制备[J]. 强激光与粒子束, 2005, 17(7): 1016. DU Shou-de, LI Bo, SHI Tao, TANG Yong-jian. Fabrication of high molar ration K2O hollow glass microsphere for laser fusion research[J]. High Power Laser and Particle Beams, 2005, 17(7): 1016.