中国激光, 2013, 40 (11): 1103007, 网络出版: 2013-10-20   

LF6铝合金激光填丝点焊工艺研究

Laser Spot Welding of LF6 Aluminum Alloy with Filler Wire
作者单位
1 哈尔滨工业大学先进焊接与连接国家重点实验室, 黑龙江 哈尔滨 150001
2 哈尔滨工业大学金属精密热加工国家级重点实验室, 黑龙江 哈尔滨 150001
摘要
针对铝合金激光点焊容易出现的问题,自建了一套精确控制送丝系统,分析铝合金激光填丝点焊的可行性,并且研究了送丝角度、延迟时间、送丝量等送丝参数的影响。研究结果表明,激光填丝点焊可以明显地改善铝合金激光点焊过程中容易出现的缺陷;送丝角度是焊丝熔化后能否稳定进入熔池的关键因素,送丝角为30°左右时,熔化焊丝进入熔池最为稳定;延迟时间过短,熔池尺寸过小时送进焊丝,易造成焊丝在试件上表面的堆积;而送丝量与焊点表面下塌的改善效果相关。
Abstract
In view of problems of laser spot welding of aluminum, a precise control wire filler is built, and the feasibility of laser spot welding of aluminum alloy with filler wire and the influences of filler wire angle, wire feed volume, delay time are analyzed. Experimental results show that the filler wire method can improve the defects of laser spot welding of aluminum. The angle of the filler wire is the key factor which influences the stability of the process of the melt wire into the pool. When the wire is feed at an angle of 30° or so, the feed process is most stable. The delay time is one of the main factors which determine the pool size. When the delay time is too short, the filler wire can be easily accumulated on the surface of the specimen. The volume of the wire feed into the pool is directly related to the improved effect of collapse.
参考文献

[1] J K Bayshore, M S Williams, Y Adonyi, et al.. Laser beam welding and formability of tailored blanks[J]. Welding Journal, 1995, 74(10): 345-352.

[2] Masashi Oikawa, Katsuhiro Minamida. Development of the laser spot welded stainless steel panel for vehicle body[C]. ICALEO, 2006. 330-336.

[3] A Matsunawa, S Katayama, H Ikeda, et al.. Effect of pulse shaping on defect reduction in pulsed laser welding[C]. ICALEO, 1992, 92(75): 547-556.

[4] 宋东风, 胡绳荪, 马力. 铝合金激光焊接技术的发展现状[J]. 电焊机, 2004, 34(9): 1-3.

    Song Dongfeng, Hu Shengsun, Ma Li. Development of laser-based welding of aluminum alloy[J]. Electric Welding Machine, 2004, 34 (9): 1-3.

[5] 梁雪平, 苏世怀. 汽车拼板的激光焊接[J]. 钢铁钒钛, 1996, 17(4): 63-69.

    Liang Xueping, Su Shihuai. Laser welding of automobile tailored blank[J]. Iron Steel Vanadium Titanium, 1996, 17(4): 63-69.

[6] 杨春燕. 激光焊接技术的应用与发展[J]. 西安航空技术高等专科学校学报, 2008, 26(5): 18-20.

    Yang Chunyan. Application and development of laser welding technology[J]. J Xi′an Aerotechnical College, 2008, 26(5): 18-20.

[7] 方志民, 谢颂京, 姚建华. 激光加工在先进制造技术中的应用[J]. 机械工程师, 2003, (8): 27-30.

    Fang Zhimin, Xie Songjing, Yao Jianhua. The application of laser machining in advances manufacturing technology[J]. Mechanical Engineer, 2003, (8): 27-30.

[8] J M Jouvard, K Girard, O Perret. Keyhole formation and power deposition in NdYAG laser spot welding[J]. Applied Physics, 2001, 34(18): 2894-2901.

[9] T W Juhl, F O Olsen. Assessment of hot crack properties of laser welded stainless steel alloys[C]. SPIE, 2003, 4831: 224-229.

[10] I Mys, M Geiger. Use of pre-pulse in laser spot welding of materials with high optical reflection[C]. SPIE, 2003, 5063: 314-318.

[11] A Matsunawa, M Mizutani, S Katayama, et al.. Porosity formation mechanism and its prevention in laser welding[J]. Welding International, 2003, 17(6): 431-437.

[12] 陈彦宾. 现代激光焊接技术[M]. 北京: 科学出版社, 2005. 96-97.

    Chen Yanbin. Laser Welding Technology[M]. Beijing: Science Press, 2005. 96-97.

[13] Xiao Rongshi, Chen Kai, Zuo Tiechuan. Influence of wire addition direction in CO2 laser welding of aluminum[C]. SPIE, 2002.

[14] A S Salminen, V P Kujanp. Effect of wire feed position on laser welding with filler wire[J]. 2003,15(1):2-10.

[15] U Dilthey, D Fuest, W Scheller. Laser welding with filler wire[J]. Optical and Quantum Electronics, 1995, 27(12): 1181-1191.

陶汪, 马轶男, 陈彦宾, 任跃冲. LF6铝合金激光填丝点焊工艺研究[J]. 中国激光, 2013, 40(11): 1103007. Tao Wang, Ma Yinan, Chen Yanbin, Ren Yuechong. Laser Spot Welding of LF6 Aluminum Alloy with Filler Wire[J]. Chinese Journal of Lasers, 2013, 40(11): 1103007.

本文已被 1 篇论文引用
被引统计数据来源于中国光学期刊网
引用该论文: TXT   |   EndNote

相关论文

加载中...

关于本站 Cookie 的使用提示

中国光学期刊网使用基于 cookie 的技术来更好地为您提供各项服务,点击此处了解我们的隐私策略。 如您需继续使用本网站,请您授权我们使用本地 cookie 来保存部分信息。
全站搜索
您最值得信赖的光电行业旗舰网络服务平台!