强激光与粒子束, 2016, 28 (8): 28081004, 网络出版: 2016-07-26  

熔石英表面杂质元素在酸蚀过程中的变化

Change of surface impurity elements in the process of acid etching on fused silica
作者单位
1 西南科技大学 材料科学与工程学院, 四川 绵阳 621010
2 中国工程物理研究院 激光聚变研究中心, 四川 绵阳 621900
摘要
为了探寻熔石英表面痕量杂质元素种类以及随HF酸蚀刻过程中的变化情况,用质量分数为1%HF酸溶液对熔石英进行长达24,48,72,96 h的静态蚀刻实验。结合飞行时间二次离子质谱(TOF-SIMS)和X射线光电子能谱(XPS)测试分析结果发现,熔石英试片表面的痕量杂质元素主要含有B,F,K,Ca,Na,Al,Zn和Cr元素,其中绝大部分都存在于贝氏层中,在亚表面缺陷层检测到有K,Ca元素。所含有的K,Na杂质元素会与氟硅酸反应生成氟硅酸盐化合物。分析表明,在HF酸蚀刻的过程中一部分杂质元素将被消除,一部分杂质元素和生成氟硅酸盐化合物会随着蚀刻液逐渐从熔石英表面向表面纵深方向扩散并被试片吸附沉积,且随着深度的加深各元素的相对含量逐渐减少。
Abstract
In order to explore the elements of trace impurities in fused silica and the change of them during HF acid etching process, the static etching experiments of 24 h, 48 h, 72 h, 96 h were performed by the mass fraction of 1% HF acid solution. The results of TOF-SIMS and XPS show that, the fused silica surface mainly contains eight trace impurity elements, including B, F, K, Ca, Na, Al, Zn, Ca, and Cr; most of these elements are in the Beiby layer, and K and Ca impurity elements are detected in the subsurface defect layer; fluosilicate salts of K, Na are generated. By analysis, during the process of HF acid etching, a part of the impurity elements will be removed, and a portion of the impurity elements and the fluosilicate salts will diffuse gradually from the surface of the fused silica to the depth with the etching liquid while some will be absorbed by fused silica surface and deposit, and the contents of them reduce gradually with the increase of the depth.
参考文献

[1] Suratwala T I, Miller P E, Bude J D, et al. HF based etching processes for improving laser damage resistance of fused silica optical surfaces [J]. Journal of the American Ceramic Society, 2011, 94(2):416-428.

[2] 苏英,周永恒,黄武,等.石英玻璃与HF酸反应动力学的研究[J].硅酸盐学报, 2004, 32(3):287-293.(Su Ying, Zhou Yongheng, Huang Wu, et al. Study on reaction kinetics between silica glasses and hydrofluoric acid. Journal of the Chinese Ceramic Society, 2004, 32(3):287-293)

[3] Verhaverbeke S, Teerlinck I, Vinckier C, et al. The etching mechanisms of SiO2 in hydrofluoric acid[J]. Journal of The Electrochemical Society, 1994, 141(10):2852-2857.

[4] 成惠峰,李要辉,吴云龙,等.硅酸盐玻璃的化学处理研究进展[J].硅酸盐通报, 2011, 39(4):827-833.(Cheng Huifeng, Li Yaohui, Wu Yunlong, et al. Research progress in wet chemical etching of silicate glass. Journal of the Electrochemical Society, 2011, 39(4):827-833)

[5] Warren L. The measurement of pH in acid fluoride solutions and evidence for the existence of (HF)2[J]. Analytica Chimica Acta, 1971, 53(1):199-202.

[6] Spierings G. Wet chemical etching of silicate glasses in hydrofluoric acid based solutions[J]. Journal of Materials Science, 1993, 28(23):6261-6273.

[7] 叶鑫,黄进,王凤蕊,等.熔石英光学元件的损伤前驱及其抑制技术[J].强激光与粒子束, 2013, 25(12):3220-3224.(Ye Xin, Huang jin, Wang Fengrui, et al. Laser damage precursors in fused silica and mitigation process. High Power Laser and Particle Beams, 2013, 25(12):3220-3224)

[8] 吴宏海,吴大清,彭金莲.重金属离子与石英表面反应的实验研究[J].地球化学, 1998(6):523-531.(Wu Honghai, Wu Daqing, Peng Jinlian. Experimental study on surface reactions of heavy metal ions with quartz. Geochimica, 1998(6):523-531)

[9] Laurence T A, Bude J D, Shen N, et al. Metallic-like photoluminescence and absorption in fused silica surface flaws[J]. Applied Physics Letters, 2009, 94:151114.

[10] Miller P, Suratwala T, Bude J, et al. Laser damage precursors in fused silica[C]//Proc of SPIE. 2009:75040X.

[11] Yoshiyama J, Genin F Y, Salleo A, et al. Effects of polishing, etching, cleaving, and water leaching on the UV laser damage of fused silica[C]//Proceedings of the Laser-Induced Damage in Optical Materials. International Society for Optics and Photonics. 1998:331-340.

[12] 杨俊,易葵,魏朝阳,等.熔石英再沉积层结构的纳米级表征和杂质分析[J].强激光与粒子束, 2014, 26:072011.(Yang Jun, Yi Kui, Wei Chaoyang, et al. Structure characterization of fused silica redeposition layer in nanoscale and analysis of impurities. High Power Laser and Particle Beams, 2014, 26:072011)

[13] 蒋晓东,郑直,祖小涛,等.亚表面杂质对熔石英激光损伤的影响[J].电子科技大学学报, 2012, 41(2):238-241.(Jiang Xiaodong, Zheng Zhi, Zu Xiaotao, et al. Distribution of inclusions in fused silica sub-surface and its influence on laser-induced damage. Journal of University of Electronic Science and Technology of China, 2012, 41(2):238-241)

[14] 王卓,吴宇列,戴一帆,等.光学材料抛光亚表面损伤检测及材料去除机理[J].国防科技大学学报, 2009, 31(2):107-111.(Wang Zhuo, Wu Yulie, Dai Yifan, et al. Detection of subsurface damage and material removal mechanism in optical polishing process. Journal of National University of Defense Technology, 2009, 31(2):107-111)

[15] Liu H, Huang J, Wang F, et al. Subsurface defects of fused silica optics and laser induced damage at 351 nm[J]. Optics Express, 2013, 21(10):12204-12217.

[16] 徐世珍,吕海兵,田东斌,等.酸蚀深度对熔石英三倍频激光损伤阈值的影响[J].强激光与粒子束, 2008, 20(5):760-764.(Xu Shizhen, Lü Haibing, Tian Dongbin, et al. effects of acid-etching depth on 355 nm laser-induced damage threshold of fused silica. High Power Laser and Particle Beams, 2008, 20(5):760-764)

殷玉春, 李玉香, 严鸿维, 袁晓东, 白阳, 郑万国. 熔石英表面杂质元素在酸蚀过程中的变化[J]. 强激光与粒子束, 2016, 28(8): 28081004. Yin Yuchun, Li Yuxiang, Yan Hongwei, Yuan Xiaodong, Bai Yang, Zheng Wanguo. Change of surface impurity elements in the process of acid etching on fused silica[J]. High Power Laser and Particle Beams, 2016, 28(8): 28081004.